Flow Coating Process Issues and Solutions in Casting Coatings
During the flow coating process of casting coating, some problems often occur. This article will analyze the causes of their formation and provide solutions. 1. Coating accumulation Reasons: Countermeasures: 2. Insufficient coating thickness Reasons: Countermeasures: Thin-walled castings 0.15mm-0.30mm Medium-sized castings 0.30mm-0.75mm Thick-walled castings 0.75mm-1.00mm Extra thick castings 1.00mm-2.00mm 3. Coating surface shedding During the assembly […]
Flow Coating Process Issues and Solutions in Casting Coatings Leer más »