wrinkle defects

Formation and prevention of wrinkle defects on the surface of ductile iron parts in lost foam casting

Wrinkle defects often appear at the last place where the molten metal flows or the “cold end” of the liquid flow, generally appearing at the top of the casting, vertical sidewalls or dead corners. The surface of this type of defect is often covered with light and shiny carbon flakes, and the depression of the […]